All data is for information only------(<---links)
PRODUCT DATA of CDA 110
MaterialCDA 110
PrecautionsTypical data from standards handbook of copper and copper alloys (CDA inc) @ Room Temperature
Chemical CompositionCu 99.9
EXPERIENCE IN PRACTICE
Equivalent DesignationsC11000; CW009A; 2.0065; E-Cu58; Cu-OFE; CDA110; C110
PHYSICAL PROPERTIES
Specific Gravity8.89 to 8.94
ELECTRICAL PROPERTIES
Electrical Volume Resistivity1.71e-8 ohm.m
THERMAL PROPERTIES
Thermal Conductivity391 W/m.K
Thermal Expansion Coefficient17 μstrain/°C
Melting Range1070 to 1080 °C
Specific Heat0.385 J/g.K
RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY
Stress Corrosion StatusHigh Resistance to SCC: Table 1
Remark:in the 37% cold rolled condition only
Data Quality: Design Data